Carbon molecular sieve uses the characteristics of sieving to achieve the purpose of separating oxygen and nitrogen. When molecular sieves adsorb impurity gases, macropores and mesopores only play the role of channels, and the adsorbed molecules are transported to micropores and submicropores, and micropores and submicropores are the volumes that really play an adsorption role. Carbon molecular sieves contain a large number of micropores that allow molecules of small kinetic size to diffuse rapidly into the pores while restricting the entry of large-diameter molecules. Due to the differences in the relative diffusion rates of gas molecules of different sizes, the components of the gas mixture can be effectively separated. Therefore, in the manufacture of carbon molecular sieves, according to the size of the molecules, the internal microporous distribution of carbon molecular sieves should be 0.28~0.38nm. In this micropore size range, oxygen can quickly diffuse into the pores through the microporous orifices, while nitrogen is difficult to pass through the microporous orifices, so as to achieve oxygen and nitrogen separation. If the pore size is too large, oxygen and nitrogen molecular sieve are easy to enter the micropores and cannot play the role of separation, and the pore size is too small, oxygen and nitrogen can not enter the micropores, nor can they play the role of separation.
Due to the limited conditions, the pore size of domestic molecular sieves is not well controlled. The micropore size distribution of carbon molecular sieves on the market is 0.3~1nm, and only Iwatani molecular sieves have achieved 0.28~0.36nm. The raw materials of carbon molecular sieve are coconut shells, coal, resin, etc., which are pulverized after processing, and then kneaded with the base material, the base material is mainly to increase the strength and prevent the material from being broken and pulverized; the second step is to activate the pores, and the activator is introduced at a temperature of 600~1000 °C, and the commonly used activators are water vapor, carbon dioxide, oxygen and their mixtures. They carry out thermochemical reactions with more active amorphous carbon atoms to expand the specific surface area and gradually form holes, and the activation time varies from 10~60min; the third step is the adjustment of pore structure, using the vapor of chemical substances: such as benzene to be deposited on the micropore wall of carbon molecular sieve to adjust the size of the pores to meet the requirements.